Friday, 30 November 2012

Cross Section Results

Our method and solutions for DPA ( Destructive physical analysis ) / Cross sections






Results by using diamond suspensions








     Results by using our product











Evaluations done on MLCC ( Multi layer ceramic capacitor )




case size : 0603 







Body type : Ceramic







Purpose of evaluations  : To get finest polishing and view under high power scope

Method :  Each mold is filled by 50 MLCC 25 Stacking and 25 Overlap were place into

                    Mold holder disc and detail process as below














Diamond sus process step







total time usage : 300 Sec

















stepprocesstime (sec)psiMethod




1200 micron Diamond12025Manual driping




290 micron diamond 12015




315 micron diamond6010




Total time usage300 sec














Our method process step







Total time usage : 120 sec

















stepprocesstime (sec)psiMethod




1A3025Auto process




2B3025




3C3025




4D3025




Total time usage120 sec














Conclusions :

















This is prove the cycle time and quality resuts are differences between 


these 2 products.

















0 comments: